LORD CoolTherm™ MD-161 conductive adhesive offers excellent electrical conductivity. It is designed for dispensing through small nozzles. CoolTherm MD-161 adhesive provides excellent adhesion to a wide variety of surfaces including silicon, silver, gold and copper. Its excellent adhesion to SiC and GaN semiconductors make CoolTherm MD-161 adhesive ideally suited for demanding LED assembly applications. Features: allows high-speed, accurate syringe dispensing of fine dots or lines; can be used with time/pressure, positive displacement or linear dispense heads; works with pin transfer equipment to precisely apply very fine dots. rapidly cures at 150°C. provides a working life of up to 5 days after loading a syringe into the dispensing equipment at room temperature. All information provided by Lord. |