MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Jilin Xingyun Chemical XY-1 Anti-oxidant for gasoline
Categories: Other Engineering Material

Material Notes: The product is of both anti-gelling agent and anti-oxidant based on amine. It is an ideal additive especially for pyrolysis or thermal gasoline. With the gasoline refined in due course, adding this product can effectively prevent olefins from oxidation to gelling formation that stability of gasoline can be improved. Asa result, the carbon accumulation can be avoided in the combustion chamber, piston top, cylinder head and other parts related. In comparison with other amine antioxidants, this product shows the characteristics of smaller dose, faster induction period and better stability, etc.

Information provided by Jilin Xingyun Chemical Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density <= 0.940 g/cc
Ash <= 0.30 %
 
Thermal PropertiesOriginal ValueComments
Solidus <= -15.0 °C
Flash Point >= 146 °C
 
Descriptive Properties
AppearanceBrown reddish
Content<0.1%
Purity>95%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PJILINX056 / 317903

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.