MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger TECAPEI™ shapes combine Ultem® PEI polymer with Ensinger's proprietary extrusion techniques for exceptional reliability, consistency, dimensional stability, and high temperature mechanical performance. FDA, USP Class VI and NSF compliant.

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin 2100 Polyetherimide (PEI) (Europe)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Polyetherimide (PEI), 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors.

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,General Purpose,High Heat Resistance,Good dimensional stability,Flame Retardant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.34 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.0 %ISO 62-1
Viscosity 9.0 cP
@Load 5.00 kg,
Temperature 360 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 140 MPaH358/30; ISO 2039-1
Tensile Strength at Break 115 MPa5 mm/min; ISO 527
Elongation at Break 4.0 %5 mm/min; ISO 527
Tensile Modulus 4500 MPa1 mm/min; ISO 527
Flexural Strength 185 MPabreak, 2mm/min; ISO 178
Flexural Modulus 4500 MPa2 mm/min; ISO 178
Izod Impact, Unnotched (ISO) 30.0 kJ/m²80*10*4; ISO 180/1U
 30.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact, Notched 7.00 kJ/m²ISO 179/2C
Taber Abrasion, mg/1000 Cycles 15CS-17, 1 kg; SABIC method
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 2.9
@Frequency 1e+6 Hz
IEC 60250
 3.0
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 15.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 27.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 34.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor 0.00090
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0025
@Frequency 1e+6 Hz
IEC 60250
 0.0046
@Frequency 2.45e+9 Hz
IEC 60250
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 100 VIEC 60112
 100 - 175 VUL 746A
 150 VIEC 60112
Hot Wire Ignition, HWI 30 - 60 sec
@Thickness >=1.50 mm
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=3.00 mm
UL 746A
 15 - 30 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 26.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Thermal Conductivity 0.240 W/m-KISO 8302
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 210 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 205 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 212 °CRate B/50; ISO 306
 217 °CRate B/120; ISO 306
 223 °CRate A/50; ISO 306
UL RTI, Electrical 170 °CUL 746B
UL RTI, Mechanical with Impact 170 °CUL 746B
UL RTI, Mechanical without Impact 170 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.410 mm
UL 94
 5VA
@Thickness >=1.90 mm
UL 94
Oxygen Index 46 %ISO 4589
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 350 - 405 °C
Zone 2 350 - 405 °C
Zone 3 360 - 415 °C
Melt Temperature 370 - 410 °CInjection Molding
Mold Temperature 140 - 180 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Precipitation Temperature 80.0 - 120 °CHopper Temperature
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82516 / 290463

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.