Description: This is a pourable 2-part addition cure silicone elastomer system. After mixing parts ‘A’ and ‘B’ in the correct proportions, the system will cure at ambient temperatures within 24 hours, but the rate of cure can be accelerated by heat. The cured rubber exhibits excellent physical and electrical properties. Key Features - Low viscosity
- Elongation > 700%
- Fast de-mold time
- Excellent flexibility
Application: Special effects.Information provided by CHT Group |