Radiation cross-linkable non-halogen flame retardant polyolefin compound Compound class: Insulation / sheathing Compound category: RDX Flame retardant: ATH Standards: SAE J1128 GXL; SAE J1127 SGX; SAE J1128 SXL; SAE J1127 STX; SAE J1128 TXL; HMC ES 91110-05; JASO D608 AESSXF; JASO D608 AEXF Typical applications: An e-beam radiation cross-linkable, halogen-free low smoke compound, offering good mechanical and electrical properties. Features: Flame retardant; Halogen-free; Low smoke; Oil resistant; Abrasion resistant; High temperature resistant; Flexible; Flexible at low temperatures Information provided by Melos |