Equiaxed beta grain structure (bcc). Highly formable, able to be cold-worked, better corrosion properties than other high strength alloys Applications: Fasteners, springs, torsion bars, foil. 3 other heat treatments of this alloy are in MatWeb. |
Ti-38-6-44; UNS R58640; Ti-3Al-8V-6Cr-4Mo-4Zr; TIMETAL 3-8-6-44 |