Function: Reclaiming agent for natural and synthetic rubber scrap Use: Aktiplast 79 is an effective reclaiming agent for natural and synthetic rubber scrap and blends thereof. Aktiplast 79 decreases the risk of cyclization and shortens the reclaiming time. Application: Rubber scrap of vulcanizates made of natural or synthetic rubber Information provided by Lanxess. |