MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC XENOY™ 1102 PC+PBT (Europe)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced

Material Notes: Unreinforced PC/polyester alloy. Excellent low temperatue impact/chemical resistance to automotive fluids.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
 1.20 g/ccASTM D792
Density 1.19 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 12 g/10 min
@Load 5.00 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 13 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 45.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 50.0 MPa50 mm/min; ISO 527
 54.0 MPa50 mm/min; ASTM D638
Elongation at Break 115 %50 mm/min; ISO 527
 150 %50 mm/min; ASTM D638
Elongation at Yield 4.5 %50 mm/min; ISO 527
Flexural Yield Strength 72.0 MPa2 mm/min; ISO 178
 82.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 1870 MPa2 mm/min; ISO 178
 1960 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 800 J/mASTM D256
 640 J/m
@Temperature -30.0 °C
ASTM D256
 690 J/m
@Temperature 0.000 °C
ASTM D256
Izod Impact, Notched (ISO) 54.0 kJ/m²80*10*4; ISO 180/1A
 44.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 52.0 kJ/m²
@Temperature 0.000 °C
80*10*4; ISO 180/1A
Charpy Impact Unnotched NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 55.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 40.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 50.0 kJ/m²
@Temperature 0.000 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 90.0 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 120 °CRate B/120; ISO 306
 155 °CRate A/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 255 - 270 °CInjection Molding
Zone 1 245 - 265 °C
Zone 2 250 - 270 °C
Zone 3 255 - 275 °C
Melt Temperature 260 - 275 °C
Mold Temperature 65.0 - 90.0 °C
Drying Temperature 110 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %
Back Pressure 0.300 - 0.700 MPa
Shot Size 50 - 80 %
Vent Depth 0.00130 - 0.00200 cm
Screw Speed 50 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10807 / 244274

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.