MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Reltek BONDiT™ B-45CC Adhesive and Sealant
Categories: Polymer; Adhesive

Material Notes: Key Properties

Excellent adhesion to low surface energy plastics without primer. Caulking and sealing dissimilar materials for harsh environments. High impact resistance. Ease of use.

Applications

Caulks and seals difficult-to-bond substrates and dissimilar materials such as UHMW polyethylene and acetal (Delrin) to steel, wood, plastics, rubber, urethane and concrete. Survives harsh environments, particularly moisture, harsh chemical, marine and sub sea. Exceptional performance as a universal caulk for industrial applications. Will cure underwater. Can be applied to oily surfaces. Ambient 24 hour or accelerated thermal cure.

Information provided by Reltek LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccA
 1.42 g/ccB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Reltek BONDiT™ B-52 Adhesive, Sealant & Potting System
Bamberger Polymers Bapolene® 4062NA Polypropylene, Injection Grade
Bamberger Polymers Bapolene® 4042 Polypropylene, Fiber/Filament Grade
Aclo Accuguard Polypropylene CP0467V0CSL Copolymer Flame Retardant Copper Stabilized

PAQREL21 / 79985

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.