MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Elkem Silgrain coarse Silicon Powder
Categories: Metal; Nonferrous Metal

Material Notes: Silgrain is a silicon powder containing min. 99% Si and can be supplied in different grades.

The main application for Silgrain® is as raw material in electronic industry (trichlorosilane - process), as alloying element in aluminum and as raw material in the ceramic industry.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 200 - 800 µm
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 0.13 - 0.25 %
Boron, B 0.0025 - 0.0035 %
Calcium, Ca 0.013 - 0.050 %
Iron, Fe 0.080 - 0.20 %
Phosphorus, P 0.0025 - 0.0035 %
Silicon, Si 99.5 %
Titanium, Ti 0.0080 - 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elkem Silgrain HQ Silicon Powder
H.C. Starck Grade AX 20 Silicon Metal Powder Si
H.C. Starck Grade AX 10 Silicon Metal Powder Si
H.C. Starck Grade AX 05 Silicon Metal Powder Si
Elkem Silgrain fine Silicon Powder

NELKEM01 / 16159

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.