MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Daikin NEOFLON® EC-6820 ETFE Coating Powder, White
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE; Modified ETFE, Unreinforced

Material Notes: Description: 0.5-5.0 mm thickness.

Processing Methods:Roto lining.

Information provided by Daikin Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.700 g/cc
Oxygen Transmission 70.0 cc-mm/m²-24hr-atmat 25°C
Nitrogen Transmission 20.0 cc-mm/m²-24hr-atmat 25°C
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.5 - 2.75
@Frequency 1000 Hz
ETFE Component; ASTM D150
 2.5 - 2.75
@Frequency 1e+6 Hz
ETFE Component; ASTM D150
Dissipation Factor 0.00040 - 0.0011ETFE Component
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0ETFE Component
Oxygen Index 31 %ETFE Component

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daikin NEOFLON® EC-6510 ETFE Coating Powder, White
AGC Fluon® TL-581 ETFE, powder

PDAIK076 / 29368

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.