Physical Properties | Original Value | Comments |
---|
Density | 1.45 - 1.78 g/cc |
| 1.40 - 1.40 g/cc @Temperature 262 - 295 °C |
Filler Content | 45.0 - 50.0 % |
Water Absorption | 0.300 - 4.80 % |
Moisture Absorption at Equilibrium | 0.170 - 2.00 % |
| 1.05 - 1.50 % @Temperature 70.0 - 70.0 °C |
Water Absorption at Saturation | 0.200 - 7.00 % |
Viscosity | 8000 - 160000 cP @Temperature 277 - 322 °C |
| 8000 - 160000 cP @Frequency 10.0 - 10000 Hz |
| 20.0 - 450 cP @Temperature 280 - 300 °C |
| 20.0 - 450 cP @Shear Rate 10.0 - 10000 1/s |
Viscosity Test | 131 - 152 cm³/g |
Viscosity Number | 105 - 150 cm³/g |
Maximum Moisture Content | 0.0200 - 0.900 |
Linear Mold Shrinkage | 0.000100 - 0.0200 cm/cm |
| 0.00100 - 0.00300 cm/cm @Temperature 80.0 - 80.0 °C |
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0125 cm/cm |
| 0.00400 - 0.00500 cm/cm @Temperature 80.0 - 80.0 °C |
Melt Flow | 1.00 - 40.0 g/10 min |
Spiral Flow | 54.0 - 536 cm |
Ash | 48.0 - 58.0 % |
|
Mechanical Properties | Original Value | Comments |
---|
Hardness, Rockwell M | 97.0 - 120 |
Hardness, Rockwell R | 98.0 - 125 |
Ball Indentation Hardness | 131 - 340 MPa |
Tensile Strength, Ultimate | 50.0 - 392 MPa |
| 65.0 - 342.669 MPa @Temperature -40.0 - 150 °C |
| 47.0 - 175 MPa @Temperature 60.0 - 180 °C |
| 47.0 - 175 MPa @Strain 0.750 - 15.0 % |
Tensile Strength, Yield | 23.5 - 265 MPa |
| 131 - 265 MPa @Temperature -20.0 - 93.3 °C |
Elongation at Break | 1.00 - 8.00 % |
| 1.80 - 8.00 % @Temperature -40.0 - 150 °C |
Elongation at Yield | 1.00 - 6.00 % |
Modulus of Elasticity | 10.2 - 22.2 GPa |
| 4.00 - 19.788 GPa @Temperature -40.0 - 150 °C |
Flexural Yield Strength | 185 - 425 MPa |
| 175 - 455.054 MPa @Temperature -40.0 - 149 °C |
Flexural Modulus | 7.90 - 106 GPa |
| 6.60 - 19.0985 GPa @Temperature -40.0 - 149 °C |
Flexural Strain at Break | 3.00 - 5.00 % |
Compressive Yield Strength | 186 - 215 MPa |
| 120 - 265 MPa @Temperature -40.0 - 80.0 °C |
Poissons Ratio | 0.330 - 0.400 |
Shear Strength | 90.0 - 105 MPa |
Secant Modulus | 5.00 - 18.0 GPa |
| 1.00 - 17.5 GPa @Temperature 60.0 - 180 °C |
| 1.00 - 17.5 GPa @Strain 0.000 - 15.0 % |
Izod Impact, Notched | 0.0600 - 6.51 J/cm |
| 1.10 - 7.36782 J/cm @Temperature -40.0 - 149 °C |
Izod Impact, Unnotched | 0.184 - 5340 J/cm |
Izod Impact, Notched (ISO) | 6.00 - 54.0 kJ/m² |
| 11.0 - 111 kJ/m² @Temperature -40.0 - -30.0 °C |
Izod Impact, Unnotched (ISO) | 75.0 - 103 kJ/m² |
| 80.0 - 96.0 kJ/m² @Temperature -30.0 - -30.0 °C |
Charpy Impact Unnotched | 0.900 J/cm² - NB |
| 0.900 J/cm² - NB @Temperature -40.0 - -20.0 °C |
Charpy Impact, Notched | 0.500 - 7.50 J/cm² |
| 0.350 - 7.50 J/cm² @Temperature -40.0 - -20.0 °C |
Dart Drop, Total Energy | 9.99 - 23.5 J @Temperature -20.0 - -20.0 °C |
| 9.99 - 23.5 J @Thickness 3.18 - 3.18 mm |
Puncture Energy | 3.60 - 23.8 J |
| 2.80 - 2.80 J @Temperature -30.0 - -30.0 °C |
Tensile Creep Modulus, 1000 hours | 5400 - 8000 MPa |
|
Electrical Properties | Original Value | Comments |
---|
Electrical Resistivity | 1.00e+9 - 1.00e+17 ohm-cm |
Surface Resistance | 1.00e+10 - 1.50e+17 ohm |
Dielectric Constant | 3.30 - 14.0 |
Dielectric Strength | 1.97 - 90.0 kV/mm |
Dissipation Factor | 0.00900 - 0.320 |
Arc Resistance | 93.0 - 180 sec |
Comparative Tracking Index | 225 - 600 V |
Hot Wire Ignition, HWI | 1.00 - 30.0 sec |
High Amp Arc Ignition, HAI | 1.00 - 120 arcs |
High Voltage Arc-Tracking Rate, HVTR | 10.0 - 50.0 mm/min |
|
Thermal Properties | Original Value | Comments |
---|
CTE, linear | 5.00 - 73.8 µm/m-°C |
| 19.0 - 20.0 µm/m-°C @Temperature 55.0 - 160 °C |
| 11.0 - 19.0 µm/m-°C @Temperature 35.0 - 55.0 °C |
| 11.0 - 19.0 µm/m-°C @Thickness 2.00 - 2.00 mm |
CTE, linear, Transverse to Flow | 40.0 - 100 µm/m-°C |
| 114 - 114 µm/m-°C @Temperature 55.0 - 160 °C |
Specific Heat Capacity | 1.30 - 1.50 J/g-°C |
| 1.87 - 1.87 J/g-°C @Temperature 262 - 295 °C |
Thermal Conductivity | 0.330 - 0.533 W/m-K |
| 0.310 - 0.310 W/m-K @Temperature 262 - 295 °C |
Melting Point | 220 - 325 °C |
Maximum Service Temperature, Air | 100 - 270 °C |
Deflection Temperature at 0.46 MPa (66 psi) | 215 - 266 °C |
Deflection Temperature at 1.8 MPa (264 psi) | 208 - 285 °C |
Deflection Temperature at 8.0 MPa | 165 - 249 °C |
Vicat Softening Point | 200 - 260 °C |
Minimum Service Temperature, Air | 100 °C |
Glass Transition Temp, Tg | 20.0 - 70.0 °C |
Decomposition Temperature | 310 °C |
UL RTI, Electrical | 65.0 - 140 °C |
UL RTI, Mechanical with Impact | 65.0 - 130 °C |
UL RTI, Mechanical without Impact | 65.0 - 140 °C |
Flammability, UL94 | HB - V-0 |
Flame Spread | 0.000 - 80.0 mm/min |
Oxygen Index | 23.0 - 32.0 % |
Glow Wire Test | 600 - 960 °C |
Ignition Temperature | 350 - 400 °C |
|
Processing Properties | Original Value | Comments |
---|
Processing Temperature | 70.0 - 315 °C |
Nozzle Temperature | 254 - 315 °C |
Die Temperature | 300 - 320 °C |
Melt Temperature | 143 - 340 °C |
Mold Temperature | 26.7 - 160 °C |
Injection Velocity | 50.8 - 80.0 mm/sec |
Drying Temperature | 26.7 - 121 °C |
Moisture Content | 0.0200 - 25.0 % |
Dew Point | -30.0 - -17.8 °C |
Injection Pressure | 3.45 - 150 MPa |
Cushion | 0.635 cm |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to go back to viewing the property data in MatWeb's normal format.