RB206MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade also features high heat distortion temperature. Applications: monolayer and multilayer bottles in the food or cosmetic industry (hot filling), and cosmetics.Information provided by Borealis AG |