Raditer® B RV 100 is a glass fiber reinforced thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properties with very good dimensional stability. Suggestions for application: Technical items with a wide range of stiffness. Information provided by Radici group. |