MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Colour Image Plastic Compound Flexiblend® PP-2100 PP, Mineral Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Product Description: Flexiblend® PP-2100 is an easy flow, thermoplastic rubber modified mineral filled polypropylene compound. This grade offers diverse automotive stringent quality requirements including hardness, mechanical and thermal properties.

Features:

  • Rubber modified
  • Mineral filled
  • Dimensional stability
  • High low temperature toughness
Uses:
  • Automotive applications
  • Trims
Forms:
  • Pellets
Processing Method:
  • Injection Molding

Information provided by Colour Image Plastic Compound Sdn Bhd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.17 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0090 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 14 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 24.0 MPaASTM D638
Elongation at Break 55 %ASTM D638
Flexural Strength 39.0 MPaASTM D790
Flexural Modulus 2450 MPaASTM D790
Izod Impact, Notched 100 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
@Thickness 4.00 mm
Unannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 180 - 190 °C
Front Barrel Temperature 190 - 200 °C
Nozzle Temperature 200 - 210 °C
Melt Temperature 210 - 220 °C
Mold Temperature 60.0 - 80.0 °C
Drying Temperature 60.0 - 80.0 °C
Dry Time 2.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCOLO120 / 266012

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.