MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay Chemicals DIGLYCEROL
Categories: Fluid

Material Notes: Diglycerol is a clear viscous liquid very similar to glycerol. It has a higher molecular weight than glycerol and is less volatile. It is water soluble and can be combined with aqueous systems.

EINECS Number: 261-605-5/CAS Number: 59113-36-9

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.276 g/cc
Viscosity 13000 cPDynamic
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 34
 
Thermal PropertiesOriginal ValueComments
CTE, linear 530 µm/m-°C
@Temperature 20.0 - 60.0 °C
Specific Heat Capacity 2.28 J/g-°C
Thermal Conductivity 0.280 W/m-K
Boiling Point 205 °C
@Pressure 0.000130 MPa
Flash Point 230 °C
Ignition Temperature 380 °CAutoignition
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.487
 
Descriptive Properties
Color<30APHA
Composition<0.5 g/kgWater
 <50 mg/kgChloride
 >90%Diglycerol
Fire point264°C
Heat of dissolution in water-52 j/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Elkem (Bluestar Silicones) BLUESIL™ FLD 47 V 3 Polydimethylsiloxanic Fluids
PBI Performance Products S26 Thermal Resistant Polybenzimidazole Solution
Syensqo (Solvay Specialty Polymers) Galden® DET PFPE Fluid
Syensqo (Solvay Specialty Polymers) Galden® HS260 PFPE VPS Fluid
Syensqo (Solvay Specialty Polymers) Galden® HS240 PFPE VPS Fluid

WSOLV154 / 147803

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.