MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE ML-1690B BLK Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ML-1690B BLK is a general purpose designed for automotive interior applications. Sarlink ML-1690B BLK is a high hardness, medium density grade suitable for injection molding. This high flow TPE exhibits improved Moldability and surface appearance.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Filled; Good Mold Release; Good Moldability; Good Processability; High Flow; Medium Density; High Hardness

Uses: Automotive Applications; Automotive Interior Parts; General Purpose; Grommets

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccISO 1183
Viscosity 133 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90
@Time 15.0 sec
Injection Molded; ISO 868
 91
@Time 5.00 sec
Injection Molded; ISO 868
 92
@Time 1.00 sec
Injection Molded; ISO 868
 90.0
@Treatment Temp. 125 °C,
Time 15.0 sec
Change in Air, 168 hr; ISO 888
 90.4
@Treatment Temp. 125 °C,
Time 1.00 sec
Change in Air, 168 hr; ISO 888
 90.9
@Treatment Temp. 110 °C,
Time 15.0 sec
Change in Air, 1008 hr; ISO 888
 90.9
@Treatment Temp. 125 °C,
Time 5.00 sec
Change in Air, 168 hr; ISO 888
 91.5
@Treatment Temp. 110 °C,
Time 5.00 sec
Change in Air, 1008 hr; ISO 888
 92
@Treatment Temp. 110 °C,
Time 1.00 sec
Change in Air, 1008 hr; ISO 888
Tensile Strength at Break 1170 psiAcross Flow, Type 1, 20 in/min; ISO 37
 1460 psiFlow, Type 1, 20 in/min; ISO 37
 1210 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
 1350 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
 1410 psi
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 1410 psi
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
Tensile Stress at Strain 711 psi
@Strain 100 %
Across Flow, Type 1, 20 in/min; ISO 37
 895 psi
@Strain 100 %
Flow, Type 1, 20 in/min; ISO 37
 780 psi
@Strain 100 %,
Treatment Temp. 110 °C
Across Flow, Type 1, Change in Air, 1008 hr; ISO 188
 796 psi
@Strain 100 %,
Treatment Temp. 125 °C
Across Flow, Type 1, Change in Air, 6.61 in; ISO 188
 1010 psi
@Strain 100 %,
Treatment Temp. 110 °C
Flow, Type 1, Change in Air, 1008 hr; ISO 188
 1030 psi
@Strain 100 %,
Treatment Temp. 125 °C
Flow, Type 1, Change in Air, 168 hr; ISO 188
Elongation at Break 580 %Flow, Type 1, 20 in/min; ISO 37
 590 %Across Flow, Type 1, 20 in/min; ISO 37
 552 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Flow, Type 1, Change in Air; ISO 188
 560 %
@Treatment Temp. 110 °C,
Time 3.629e+6 sec
Across Flow, Type 1, Change in Air; ISO 188
 568 %
@Treatment Temp. 125 °C,
Time 605000 sec
Flow, Type 1, Change in Air; ISO 188
 642 %
@Treatment Temp. 125 °C,
Time 605000 sec
Across Flow, Type 1, Change in Air; ISO 188
Tear Strength 220 pliFlow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
 270 pliAcross Flow, Method Ba, Angle (Unnicked), 20 in/min; ISO 34-1
Compression Set 38 %
@Temperature 22.8 °C,
Time 79200 sec
Type 1; ISO 815
 62 %
@Temperature 70.0 °C,
Time 79200 sec
Type 1; ISO 815
 76 %
@Temperature 90.0 °C,
Time 252000 sec
Type 1; ISO 815
 100 %
@Temperature 125 °C,
Time 252000 sec
Type 1; ISO 815
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 340 - 380 °F
Middle Barrel Temperature 350 - 390 °F
Front Barrel Temperature 360 - 400 °F
Nozzle Temperature 370 - 410 °F
Melt Temperature 370 - 410 °F
Mold Temperature 77.0 - 150 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 50.0 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1116 / 237607

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.