MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Parylene Coating Services N Poly (P-Xylylene)
Categories: Polymer; Thermoplastic; Poly (P-Xylylene)

Material Notes: Monomer is para-xylylene. Parylene N has a lower coefficient of friction and therefore is recommended where lubricity is needed. Parylene N exhibits a slight haze at thicknesses over 5 microns.

Parylene is a generic name for poly-para-xylylene polymers used as conformal coatings in protective applications.

The coating process exposes objects to the gas-phase monomer at low pressure. Through vacuum deposition, Parylene condenses on the surface in a polycrystalline fashion, providing a coating that is truly conformal and pinhole free.

Compared to liquid processes, the effects of gravity and surface tension are negligible -- so there is no bridging, thin-out, pinholes, puddling, run-off or sagging. And, since the process takes place at room temperature, there is no thermal or mechanical stress on the object.

Parylene is physically stable and chemically inert within its usable temperature range. Parylene provides excellent protection from moisture, salt spray, corrosive vapors, solvents, airborne contaminants and other hostile environments.

Property data obtained following ASTM methods. Information provided by Parylene Coating Services, Inc. (PCS)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/cc
Water Absorption 0.010 %0.019 inches; 24 hrs.
Moisture Vapor Transmission 1.50 cc-mil/100 in²-24hr-atm37°C; 90% RH
Oxygen Transmission 30.0 cc-mil/100 in²-24hr-atm23°C
Nitrogen Transmission 7.70 cc-mil/100 in²-24hr-atm23°C
Carbon Dioxide Transmission 214 cc-mil/100 in²-24hr-atm23°C
Hydrogen Sulfide Transmission 795 cc-mil/100 in²-24hr-atm23°C
Sulfur Dioxide Transmission 1.89 cc-mil/100 in²-24hr-atm23°C
Chlorine Transmission 74.0 cc-mil/100 in²-24hr-atm23°C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 6500 psi
Tensile Strength, Yield 6300 psi
Elongation at Break 40 %
Elongation at Yield 2.5 %
Tensile Modulus 2.40 GPa
Coefficient of Friction, Dynamic 0.25
Coefficient of Friction, Static 0.25
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+17 ohm-cm50% RH
Surface Resistance 1.00e+15 ohm50% RH
Dielectric Constant 2.65
@Frequency 60 Hz
 2.65
@Frequency 1000 Hz
 2.65
@Frequency 1e+6 Hz
Dielectric Strength 7000 V/milShort Time; 1 mil
Dissipation Factor 0.00020
@Frequency 60 Hz
 0.00020
@Frequency 1000 Hz
 0.00060
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 69.0 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 0.120 W/m-K
Melting Point 410 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.661

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Specialty Coating Systems Parylene N Poly (P-Xylylene) Coating
Parylene Coating Services C Poly (P-Xylylene)
Parylene Coating Services D Poly (P-Xylylene)
Specialty Coating Systems Parylene C Poly (P-Xylylene) Coating
Specialty Coating Systems Parylene D Poly (P-Xylylene) Coating

PPARYLN / 55913

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.