MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Röchling GLASTHERM HT200 Insulation Sheet
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: HT200 features:
  • High Hot Compressive Strength
  • Low Thermal Conductivity
  • Oil and Moisture Resistant
  • Reduces Heat Loss
  • Helps Control Temperature
  • Faster Mold Startup
Designed for reducing heat losses from plastic and zinc die cast molds with operating temperatures up to 550º F. Its thermal insulating capability provides faster startups and increased operating efficiency while its high strength provides long service life. It is asbestos-free and rugged to withstand mechanical abuse during installation. It is easily cut and machined with standard metal working equipment. Diamond cutting tools are recommended for long life.

Information provided by Red Seal Electric.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.97 g/ccASTM D-792
Water Absorption 0.2 %% by wt.; ASTM D-570
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 31000 psiASTM D-790
Compressive Strength 17000 psi
@Temperature 288 °C
ASTM D-695
 18000 psi
@Temperature 200 °C
ASTM D-695
 27000 psi
@Temperature 150 °C
ASTM D-695
 49000 psi
@Temperature 23.9 °C
ASTM D-695
Compressive Modulus 1.80e+6 psiASTM D-695
Izod Impact, Notched 8.00 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 50.0 kV/inS/T in Air
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.1 µm/m-°C
@Temperature 20.0 °C
Across Surface; ASTM D-696
 116.2 µm/m-°C
@Temperature 20.0 °C
Across Thickness; ASTM D-696
Thermal Conductivity 0.270 W/m-KASTM C-177
Maximum Service Temperature, Air 412 °FContinuous
 550 °F
Flammability, UL94 HB
@Thickness 2.40 mm
 
Descriptive Properties
Standard ColorWhite or Green

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Galden® HT200 PFPE Heat Transfer Fluid

PGLASW6z / 137228

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.