MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
3M Cushion-Mount™ E1060H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion
Categories: Polymer; Adhesive

Material Notes: 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for combination printing, process printing, solids and line work. 3M now offers a range of 40 and 60 mil cushioned plate mounting tapes for flexographic printing needs.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.450 g/cc
Thickness 4.50 milFilm Liner
 62.0 milTape
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 15.0 psi10% Compression, Deflection
 25.0 psi25% Compression, Deflection
Peel Strength 2.1875 pliLinered side-Photopolymer, Adhesion; ASTM D3330
 3.125 pliNon-linered side-Composite Sleeve, Adhesion; ASTM D3330
 3.4375 pliNon-linered side-Urethane-B, Adhesion; ASTM D3330
 3.75 pliNon-linered side-Stainless Steel, Adhesion; ASTM D3330
 4.0625 pliNon-linered side-Polyester, Adhesion; ASTM D3330
 4.375 pliNon-linered side-Urethane-A, Adhesion; ASTM D3330
 
Descriptive Properties
LinerStandard White Foam

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM33947 / 168694

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.