Hostacom TKS736D NATRL medium melt flow, 990 MPa flexural modulus, precolored, UV-stabilized thermoplastic elastomeric olefin (TEO) resin has an excellent combination of stiffness, impact resistance and processability. It is typically used for outdoor applications that require high durability. Applications: Automotive Parts, Exterior Automotive ApplicationsInformation provided by LyondellBasell. |