MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Purell RP320M Polypropylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Purell RP320M is a controlled rheology medium modified polypropylene random copolymer. It does not contain slip or anti-blocking additives. Purell RP320M is typically used for manufacturing of un-oriented cast films. Customer report lamination, textile and packaging of foodstuffs as typical applications. Purell RP320M exhibits good processability, and that films produced with Purell RP320M exhibits high clarity and gloss, softness and good heat weldability. Applications: Caps & Closures (Healthcare), Healthcare Applications, Medical Film.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183-1
Melt Flow 8.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 25.0 MPaISO 527-1,-2
Elongation at Break >= 50 %ISO 527-1,-2
Elongation at Yield 13 %ISO 527-1,-2
Tensile Modulus 850 MPaISO 527-1,-2
Charpy Impact, Notched 2.00 kJ/m²
@Temperature 0.000 °C
ISO 179-1/1eA
 7.00 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 135 °CA50; ISO 306
 
Descriptive Properties
Processing MethodCast Film, Injection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem RP250 Polypropylene Random Copolymer
Bamberger Polymers Bapolene® 5063C Polypropylene, Injection Grade
Dow 6D20 Polypropylene Random Copolymer Resin
Flint Hills P9R6K-054A Random Copolymer Polypropylene
I. Stern 2335C Prime Clarified Random Copolymer Polypropylene

PEQT8643 / 220277

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.