System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC LEXAN™ PC2200R PC (Asia)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
Material Notes:
PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. It is available exclusively at www.sabicpc.com
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.20
g/cc
ASTM D792
Density
1.20
g/cc
ISO 1183
Water Absorption
0.35 %
23°C/sat; ISO 62
Moisture Absorption at Equilibrium
0.35 %
ASTM D570
Linear Mold Shrinkage, Flow
0.0050
-
0.0070
cm/cm
SABIC method
0.0050
-
0.0070
cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow
21
g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm³/10 min; ISO 1133
22
g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell R
120
ISO 2039-2
120
ASTM D785
Tensile Strength, Yield
63.0
MPa
50 mm/min; ASTM D638
63.0
MPa
50 mm/min; ISO 527
Elongation at Break
>= 70 %
50mm/min; ISO 527
>= 70 %
50mm/min; ASTM D638
Elongation at Yield
6.0 %
50 mm/min; ISO 527
6.0 %
50 mm/min; ASTM D638
Tensile Modulus
2350
MPa
1mm/min; ISO 527
2350
MPa
50 mm/min; ASTM D638
Flexural Yield Strength
90.0
MPa
1.3 mm/min, 50 mm span; ASTM D790
90.0
MPa
2 mm/min; ISO 178
Flexural Modulus
2300
MPa
1.3 mm/min, 50 mm span; ASTM D790
2300
MPa
2 mm/min; ISO 178
Izod Impact, Notched
640
J/m
ASTM D256
Izod Impact, Unnotched
NB
ASTM D4812
Izod Impact, Notched (ISO)
65.0
kJ/m²
80*10*3; ISO 180/1A
12.0
kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO)
NB
80*10*3; ISO 180/1U
NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Dart Drop, Total Energy
55.0
J
peak; ASTM D3763
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+15
ohm-cm
ASTM D257
>=
1.00e+15
ohm-cm
IEC 60093
Dielectric Constant
3.0
@Frequency 1e+6 Hz
IEC 60250
3.0
@Frequency 60 Hz
IEC 60250
3.0
@Frequency 1e+6 Hz
ASTM D150
3.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength
27.0
kV/mm
@Thickness 1.60 mm
IEC 60243-1
27.0
kV/mm
@Thickness 1.60 mm
ASTM D149
Dissipation Factor
0.0010
@Frequency 60 Hz
ASTM D150
0.0010
@Frequency 60 Hz
IEC 60250
0.010
@Frequency 1e+6 Hz
IEC 60250
0.010
@Frequency 1e+6 Hz
ASTM D150
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
70.0
µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
70.0
µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
Thermal Conductivity
0.200
W/m-K
ASTM C177
0.200
W/m-K
ISO 8302
Hot Ball Pressure Test
125
°C
IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi)
133
°C
Flatw 80*10*4 sp=64mm; ISO 75/Bf
133
°C
@Thickness 3.20 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
122
°C
Flatw 80*10*4 sp=64mm; ISO 75/Af
122
°C
@Thickness 3.20 mm
ASTM D648
Vicat Softening Point
140
°C
Rate B/50; ISO 306
140
°C
Rate B/50; ASTM D1525
Flammability, UL94
V-2
@Thickness 1.60 mm
UL 94
Optical Properties
Original Value
Comments
Refractive Index
1.586
ISO 489
1.586
ASTM D542
Haze
<= 0.80 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible
88 - 90 %
@Thickness 2.54 mm
ASTM D1003
Processing Properties
Original Value
Comments
Processing Temperature
60.0
-
80.0
°C
Hopper Temperature
Nozzle Temperature
270
-
290
°C
Injection Molding
Zone 1
260
-
280
°C
Zone 2
270
-
290
°C
Zone 3
280
-
300
°C
Melt Temperature
280
-
300
°C
Mold Temperature
80.0
-
100
°C
Drying Temperature
120
°C
Injection Molding
Dry Time
2.00
-
4.00
hour
Injection Molding
Moisture Content
0.020 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABI10558 / 244025
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.