MA300-M is injection a molding aesthetic resin. MA300-M has many properties: (1) anti-scratch (2) high gloss (G60°>85) (3) bright color (4) UV stability (5) light transmittance (6) recycling. MA300-M is mainly used in appearance items of household appliance, etc.Information provided by Shanghai Kumho Sunny Plastics co, Ltd |