MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Taiwan PU CPU-49-U300A-A Spraying Pure Polyurea Elastomer
Categories: Polymer; Thermoset; Polyurethane, TS

Material Notes: Key features:
  • Hardness: ? 40 Shore D
  • Mixing ratio: 1:1 by volume
  • 100% solid content
  • Fast curing & easy to use
  • No VOCs
Description: This product is 100% solid, two component, high performance polyurea elastomer based on aromatic MDI and Amine Polyol. Its characteristics include outstanding tear, abrasion resistance, high elongation and adhesion. Also, it provides outstanding alkali, acid resistance and chemical resistance. Spraying Polyurea Elastomer CPU-49-U300A-A/B displays extremely fast cure times and shrinkage resistance.

Application:

  • Packing lot flooring.
  • Foam coatings.
  • Pipeline coatings.
  • Protecting for building.
  • Secondary containment.
  • Bridge coatings.
  • Corrosion protection for steel.
Characteristics:
  • High thermal stability, chemical resistance, waterproof properties.
  • Corrosion resistance & aging resistance.
  • Outstanding physical performance including abrasion resistance, elasticity, flexibility.
  • Easy application.
  • Environmentally friendly, no VOCs, 100% solid.

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 - 1.15 g/cc
Viscosity 300 - 400 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 40
Tensile Strength >= 80.0 kg(f)/cm²
Elongation at Break >= 300 %
Tear Strength >= 75.0 kg(f)/cm
 
Processing PropertiesOriginal ValueComments
Cure Time 12.0 secTack free time
 24.0 hourFull Dry
Gel Time 0.167 min
Shelf Life 12.0 Month
 
Descriptive Properties
Mixing ratio100by volume
 110by weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTAIWPU033 / 305763

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.