MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Kolon SPESIN® KP212G30V0S Polybutylene Terephthalate (PBT), 30% Glass Fiber
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: PBT + GF30%, flame retardant, injection molding.

Information provided by Kolon Plastic, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.68 g/ccASTM D792
Water Absorption 0.060 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0050 - 0.011 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 115 MPa
@Thickness 3.20 mm
5 mm/min; ASTM D638
Flexural Strength 185 MPa
@Thickness 3.20 mm
5 mm/min; ASTM D790
Flexural Modulus 8600 MPa
@Thickness 3.20 mm
5 mm/min; ASTM D790
Izod Impact, Notched 55.0 J/m
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 224 °C20°C/min; ASTM D1525
Deflection Temperature at 1.8 MPa (264 psi) 210 °CASTM D648
Flammability, UL94 V-0
@Thickness 0.750 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 230 - 250 °C
Middle Barrel Temperature 240 - 260 °C
Front Barrel Temperature 245 - 270 °C
Nozzle Temperature 245 - 265 °C
Mold Temperature 60.0 - 100 °C
Drying Temperature 100 - 120 °C
@Time 10800 - 18000 sec
Dehumidifying Dryer
Moisture Content <= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKOKZ749 / 255760

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.