MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
3M 7777 Polypropylene Label Material
Categories: Polymer; Adhesive

Material Notes: 3M™ Polypropylene Label Material 7777 is a durable material that offers good thermal stability and moisture resistance. This label material utilizes 3M™ Permanent Acrylic Adhesive, which is designed for use in various applications.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 0.900 milAdhesive
 2.60 milFacestock
 3.20 milLiner
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 2.20 pli180° Peel, 12"/min., 1" wide sample; TLMI Method
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 49.0 °C
Minimum Service Temperature, Air 5.00 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature >= -29.0 °CApplication
 <= 125 °CApplication
Shelf Life 24.0 Month
 
Descriptive Properties
Adhesive TypePermanent acrylic
Liner50# super calendered kraft sheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Colorite Polymers 7777 Non-Phthalate 77 Series Vinyl Compound
DuPont Mobility and Materials Kalrez® AeroSeal™ 7777 Fluoroelastomer
Axiall 7777 Rigid PVC, Extrusion

PMM33737 / 168484

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.