MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Zortrax Z-ULTRAT Plus Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: Z-ULTRAT Plus is a material which combines high impact resistance and improved adhesion between individual layers in models. Its qualities provide enhanced durability of 3D printed items, allowing you to create complex mechanisms and strong end-use parts. Z-ULTRAT Plus is based on ABS and therefore is a perfect alternative for this widely known and used by the industry thermoplastic. This material becomes the best choice for many areas, including automotive or manufacturing, where prototypes require high tolerance during impact tests.

Information provided by Zortrax

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.141 g/ccISO 1183-3:2003
Melt Flow 108.1 g/10 min
@Load 5.00 kg,
Temperature 260 °C
ISO 1133:2006
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 67ISO 868:1998
Tensile Strength at Break 31.32 MPaISO 527:1998
Tensile Strength 32.02 MPaISO 527:1998
Elongation at Break 3.44 %ISO 527:1998
Elongation at Yield 3.41 %ISO 527:1998
Flexural Strength 51.7 MPaISO 178:2011
Flexural Modulus 1510 MPaISO 178:2011
Izod Impact, Notched (ISO) 7.71 kJ/m²ISO 180:2004
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 70.19 °CISO 11357-3:2014

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZORT008 / 281887

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.