MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Raschig Group MELOPLAS® 183 MF
Categories: Polymer; Thermoset; Melamine; Melamine-Phenolic Copolymer; Phenolic

Material Notes: Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 181, high surface hardness, good mechanical strength and heat resistance, good abrasion and UV stability. Self-extinguishing (V-0/1,6 according to UL 94), UL-listed in all colors. Free of halogens and toxic heavy metals. Supervised according ISO 14529-3, DIN 7708: MP 183, ISO 800: MPF C10, ISO 14529-3: MP (LD20+MD30) -(LD30+MD20). Forms: Low dust granulate packed in moisture resistant bags. Standard bag size: 25 kg palletized in 1.000 kg loads or big-bags. Processing: Injection and compression, Applications: Molded parts in electrical engineering.

Information provided by the Raschig Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.60 - 1.70 g/ccISO 1183
Apparent Bulk Density 0.550 - 0.750 g/ccISO 60
Water Absorption <= 1.7 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm(longitudinal) Compression; ISO 2577
 0.0070 - 0.011 cm/cm(longitudinal) Injection; ISO 2257
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 40.0 - 65.0 MPaCompression; ISO 527
 50.0 - 80.0 MPaInjection; ISO 527
Modulus of Elasticity 5.00 - 8.00 GPaInjection and Compression; ISO 527
Flexural Strength 70.0 - 100 MPaCompression; ISO 178
 90.0 - 120 MPaInjection; ISO 178
Flexural Modulus 8.00 - 9.00 GPaInjection and Compression; ISO 178
Compressive Strength 200 - 250 MPaISO 604
Charpy Impact Unnotched 0.500 - 0.800 J/cm²
@Temperature 23.0 °C
Compression; ISO 179/ 1eU
 0.700 - 1.00 J/cm²
@Temperature 23.0 °C
Injection; ISO 179/ 1eU
Charpy Impact, Notched 0.120 - 0.180 J/cm²
@Temperature 23.0 °C
Compression; ISO 179/ 1eA
 0.130 - 0.200 J/cm²
@Temperature 23.0 °C
Injection; ISO 179/ 1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 - 1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+10 - 1.00e+11 ohmIEC 60093
Dielectric Constant 7.0 - 9.0
@Frequency 1e+6 Hz
IEC 60250
 11 - 16
@Frequency 100 Hz
IEC 60250
Dielectric Strength 20.0 - 25.0 kV/mmIEC 60243-1
Dissipation Factor 0.030 - 0.050
@Frequency 1e+6 Hz
IEC 60250
 0.30 - 0.50
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.0 - 35.0 µm/m-°C
@Temperature 50.0 - 100 °C
ISO 11359-2
Thermal Conductivity 0.400 - 0.500 W/m-KASTM E1461
Maximum Service Temperature, Air 135 °C20,000 h; IEC 60216/T1
 160 °C< 50 h; IEC 60216/T1
Deflection Temperature at 1.8 MPa (264 psi) 155 - 180 °CInjection and Compression; ISO 75-A
Deflection Temperature at 8.0 MPa 110 - 130 °CInjection and Compression; ISO 75-C
Flammability, UL94 V-0
@Thickness 1.50 mm
Shrinkage 1.0 - 1.5 %
@Temperature 110 °C,
Time 605000 sec
Post-shrinkage; ISO 2577
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 15.0 - 25.0 °C
 
Descriptive Properties
Arc resistance5 StufeASTM D495
Glow wire ignitability test900/1IEC 60695 2-13
Glow-wire flammability test960/1IEC 60695 2-12
Water Absorption<100 mgISO 62; 24h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Free-Cutting Brass, UNS C36000
Chengdu Polyster MCA Melamine Cyanurate
Oceanchem Group Melamine Cyanurate (MCA)
Perstorp Compounds Aminel FX Melamine
Raschig Group MELOPAS® 2010 MF Melamine

PRASCH32 / 65317

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.