MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Konson TBSI Rubber Accelerator
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Chemical Name: N,N-bis(1,3-benzothiazol-2-ylsulfanyl)-2-methylpropan-2-amine

Molecular Formula: C18H17N3S4

CAS#: 3741-80-8

Description: TBSI can replace NOBS which is carcinogenic and does not generates the nitrosamines as primary amine-based accelerator . The rubber added with TBSI can obtain good scorch safety and lower vulcanization rate, and show good curing reversion resistance, high modulus and lower heat generation, which optimizes adhesion between rubber and brass coated steel cord. Its physical properties and dynamic properties of cured rubber are similar with NOBS and DCBS cured rubber. It can also replace the blend of primary amine accelerator TBBS or CBS and scorch retarder CTP and be used alone, which makes it ideal for thick articles requiring a balanced cure and provides improved reversion resistance both during extended cure times at elevated temperatures and during product service life.

Dosage: NR: 0.5 – 1.5 phr IR: 0.5 – 1.5 phr SBR: 0.5 – 1.5 phr NBR: 0.5 – 1.5 phr HNBR: 0.5 – 1.5 phr

Applications: This product will not generate the carcinogenic substance- nitrosamines which be known more secure from NOBS, DIBS and DCBS under the same operation temperature. It can be used in NR, SBR, Butadiene rubber and IR. Especially apply to the furnace black sizing material with strong acid, showing the much better activity than CBS and NOBS.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Molecular Weight 403.61 g/mol
Ash <= 0.50 %
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 128 °CInitial
 
Descriptive Properties
AppearanceLight-white powder
Heat Loss<0.5%
Sieve residue<0.1%150µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKONS054 / 256099

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.