Description: BRALEN RB 03-23 is a general purpose grade of low density polyethylene. It is characterized by high environmental stress cracking resistance and very good mechanical properties. This grade is additives free. Applications: BRALEN RB 03-23 is designed for production of heavy duty and shrink films. It is well suited for blow molding of various containers, bottles, pipes, sheets and profiles extrusion and for injection molding. Recommended film thickness is 0.07 to 0.25 mm. (1) Density has been measured on pressed mould specimen according to internal method. (2) Film properties tested using 70 µm thick blown film extruded at a blow up ratio 2.5:1. (3) Typical properties measured on standard injection molded test specimen according to ISO 294-1. Information provided by Molgroup Chemicals |