MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Mid-Mountain Materials HYTEX® 2500 Ceramic Fiber Industrial Textile
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: HYTEX® 2500 Ceramic Fiber Industrial Textiles are exceptionally effective high temperature textile products capable of withstanding continuous temperatures up to 2500ºF (1370ºC). Manufactured from ceramic fiber yarn with no supportive carrier fibers, these products retain strength, flexibility and molten metal resistance at higher temperatures than most other refractory textile materials. Low thermal conductivity and high electrical resistivity makes HYTEX® 2500 products highly efficient as high temperature thermal and electrical insulation. HYTEX® 2500 textiles are compatible with silicone, epoxy, phenolic, polyester, and polyimide matrix materials. Fire barriers constructed from HYTEX® 2500 products are lighter weight than metallic materials and have successfully passed FAA 2000ºF (1095ºC) 15-minute flame penetration tests. HYTEX® 2500 products can be supplied with special densities, constructions, and pressure-sensitive adhesive backing. HYTEX® 2500 products are fabricated in various forms and shapes to customer specifications utilizing thermally compatible sewing thread.

Information provided by Mid-Mountain Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 1795 °C
Maximum Service Temperature, Air 2500 °FContinuous
 2800 °FShort term
 
Component Elements PropertiesOriginal ValueComments
Al2O3 70 %
 
Descriptive Properties
Abrasion ResistanceFair to Good
Acid ResistanceGood
Alkali ResistanceFair
ColorWhite
Solvent ResistanceExcellent
Sunlight and Aging ResistanceExcellent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMID01b / 141228

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.