MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastics Group Polifil® GFPC-30 30% Glass-Reinforced Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 30% Glass Filled

Material Notes: Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycarbonate line an excellent choice for electrical, appliance and hardware applications. Standard processing techniques are applicable.

Information provided by The Plastics Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccASTM D792
Filler Content 30 %ASTM D2584
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
@Thickness 1.59 mm
ASTM D955
Melt Flow 12 - 20 g/10 min300/1.2; May be specified; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 92ASTM D785
Tensile Strength at Break 18800 psiASTM D638
Elongation at Break 4.0 %ASTM D638
Tensile Modulus 1.25e+6 psiASTM D790
Flexural Strength 22700 psiASTM D790
Flexural Modulus 1.15e+6 psiTangent; ASTM D790
Izod Impact, Notched 2.00 ft-lb/inAt 73°F; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 295 °FASTM D648
Flammability, UL94 HB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Oxford Polymers 30GF 30% Glass Fiber Filled Polycarbonate for Injection Molding
Omni Plastics OmniTech™ PC GR30 Glass Reinforced Polycarbonate
PTS Tristar® PC-30GFR 30% Glass Reinforced Polycarbonate
Chevron Phillips Xtel® XK2040 Polyphenylene Sulfide Alloy
Arkema Kynar® 705 PVDF

PPOLI040 / 56944

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.