MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SMAC SMACMOUNT® 2112S 03 Damping Material
Categories: Other Engineering Material

Material Notes: Specifications - Shock & vibration insulation for:
  • Aircraft avionics components & subassemblies
  • Missile electronics
  • Vehicular electronics requiring vibration isolation
Advantages :
  • Bushing style mount
  • Countersunk for lowest installed height
  • Can be pre-loaded to vary natural frequency
  • Axial to radial stiffness ratio of approx. 1:1

    Information provided by SMAC MontBlac Groupe Technologies

  • Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Descriptive Properties
    Load<4.5 kg
     10 kg1 mm, Static Deflection
     22 kg2 mm, Static Deflection
     3 kg40 Hz, Natural frequency
     4.1 kg23 Hz, Natural frequency
     50 kg3 mm, Static Deflection

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    SMAC SMACTANE® 60 1114S- N01 Damping Material
    SMAC SMACTANE® SP Damping Material
    SMAC SMACWRAP® ST Damping Material, 1 mm
    SMAC SMACMOUNT® 2112S Damping Material
    SMAC SMACFOAM® 1250S-11 Damping Material

    PZSMAC025 / 146141

    Specialty Compounds RTP Company

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.