MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cabot CAB-O-SIL® CLARUS™ 3140 Fumed Silica
Categories: Polymer

Material Notes: Product highlights: CAB-O-SIL® CLARUS™ 3140 fumed silica offers a wide range of properties. It enables transparency, reinforcement, and ease of compounding to final products. CAB-O-SIL® CLARUS™ 3140 fumed silica is especially suited for high transparency elastomer preparation with silicone gum as a matrix. This product allows for easy dispersion by conventional compounding mixers. It is suitable for high temperature vulcanized (HTV) silicone elastomer formulations that require excellent transparency and reinforcement. It also enables excellent aging resistance at a wide temperature range between -40°C and 200°C.

Key applications: CAB-O-SIL® CLARUS™ 3140 fumed silica is suitable for use in high transparency silicone elastomers.

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Mooney Viscosity 33.75ML (1+4)
 37.75Mooney peak
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 8.48 MPa
Elongation at Break 3490 %
 
Optical PropertiesOriginal ValueComments
Haze 54.8 %
Transmission, Visible 65.8 %
 
Descriptive Properties
Product FormFluffy Powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCABOT009 / 315744

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.