MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Teknor Apex Chemlon® 60CF6 Nylon 6, 20% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Carbon Fiber Filled

Material Notes: Notes: 60CF6 is a 30% carbon fiber grade of nylon 6. It offers outstanding strength and stiffness-coupled with low density and improved electrical conductivity of molded parts. It is suitable for applications such as bearings and mechanical parts.

Availability: Europe

Fillers/Reinforcement: Carbon Fiber, 30% Filler by Weight

Features: High Stiffness; High Strength; Low Density

Uses: Bearings; Machine/Mechanical Parts

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.28 g/ccISO 1183
Moisture Absorption at Equilibrium 2.1 %50% RH; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 30500 psiISO 527-2
Elongation at Break 3.5 %ISO 527-2
Tensile Modulus 2.47e+6 psiISO 527-2
Flexural Strength 43500 psiISO 178
Flexural Modulus 2.68e+6 psiISO 178
Izod Impact, Notched (ISO) 2.40 ft-lb/in²ISO 180/A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) >= 392 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) >= 392 °FUnannealed; ISO 75-2/A
Flammability, UL94 HB
@Thickness 1.52 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 482 - 536 °F
Middle Barrel Temperature 482 - 536 °F
Front Barrel Temperature 482 - 536 °F
Melt Temperature 482 - 536 °F
Mold Temperature 158 - 194 °F
Drying Temperature 176 °F
Dry Time 2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0373 / 236864

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.