System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Zell-Metall Engineering Plastics Zellamid 1100 MO at 50% RH
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, MoS2 Filled
Material Notes:
Improved sliding and self-lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.
Color: black
Applications: For conveyor screws
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.15
g/cc
Dry Density
Moisture Absorption at Equilibrium
2.5 - 3.0 %
50% RH
Water Absorption at Saturation
6.0 - 7.0 %
23°C
Mechanical Properties
Original Value
Comments
Hardness, Shore D
78 - 80
DIN 53505
Tensile Strength at Break
70.0
-
72.0
MPa
DIN 53455
Elongation at Break
30 - 60 %
DIN 53455
Tensile Modulus
2.80
GPa
DIN 53457
0.500
GPa
@Temperature 100 °C
DIN 53457
Charpy Impact, Notched
4.50
-
8.50
J/cm²
DIN 53453
Coefficient of Friction
0.050 - 0.10
to steel, added lubrication
0.30 - 0.35
to steel, no lubrication; ISO/DTR 7147
Tensile Creep Modulus, 1000 hours
<=
500
MPa
DIN 53444
Electrical Properties
Original Value
Comments
Volume Resistivity
3.00e+12
-
5.00e+12
ohm-cm
DIN 53482
Surface Resistance
1.00e+10
-
3.00e+10
ohm
DIN 53482
Dielectric Constant
12
@Frequency 1e+6 Hz
DIN 53483
Dielectric Strength
15.0
-
20.0
kV/mm
DIN 53481
Dissipation Factor
0.15
@Frequency 1e+6 Hz
DIN 53483
Comparative Tracking Index
600
V
KV Method; DIN 53480
Thermal Properties
Original Value
Comments
CTE, linear
80.0
µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity
1.67
J/g-°C
Thermal Conductivity
0.280
W/m-K
DIN 52612
Melting Point
220
°C
Maximum Service Temperature, Air
100
-
120
°C
long time operation
120
-
140
°C
medium time operation
160
°C
a few hours operation
Minimum Service Temperature, Air
-40.0
°C
Flammability, UL94
HB
Descriptive Properties
Time yield limit
up to 8.5
s1/1000; DIN.53444
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Zell-Metall Engineering Plastics Zellamid 250 (PA6.6)
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH
Zell-Metall Engineering Plastics Zellamid 1100 MO
PZELL19 / 72948
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.