MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis CC7209 Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: CC7209 is an extrusion coating grade especially designed for seal-peel applications. It gives smooth and easy peel when sealed against itself and PE. CC7209 provides also good adhesion to various substrates, particularly to aluminum. The recommendation is to mix it with standard LDPE with the ratio 1:1 In this mixture processing like standard LDPE can be applied. The material must be pre-dried but there can be still a slight risk for filter blocking and filler agglomeration. Applications: extrusion coated seal-peel structures, tie layer for aluminum in extrusion coated/laminated, structures, and food packaging. CC7209 contains finely dispersed filler but no other additives.

Information provided by Borealis AG

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.15 g/ccISO 1183
Melt Flow 5.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis BS2581 High Density Polyethylene for Blow Molding
Borealis FA7229 Low Density Polyethylene
Borealis FT3200 Low Density Polyethylene
Borealis FS1470 High Density Polyethylene
Borealis FA3220 Low Density Polyethylene

PBOREA397 / 108656

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.