MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Liveo™ Q7-2243 LVA, Simethicone USP Antifoam
Categories: Polymer; Thermoset; Silicone

Material Notes: Low-volatile silicone antifoam for use in medical and pharmaceutical applications requiring foam suppression or inhibition.

Information provided by DuPont. This was previously a Dow Corning product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.975 g/ccfor silicone fluid only; ASTM D 4052
Viscosity 570 cP
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.404for silicone fluid only
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Compliance PropertiesOriginal ValueComments
FDA YesFood Contact per FDA 21 CFR
 
Component Elements PropertiesOriginal ValueComments
SiO2 4.0 - 7.0 %PhEur 1470
 
Descriptive Properties
BasisPDMS + SiO2
ColorGray
Defoaming performance< 15 s20 PPM; PhEur 1470
Heavy metals content< 5 ppm
Polymer((Si)+Compound)
Volatility (%)< 14h at 200°C; PhEur 1470

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX4716 / 256165

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.