MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Geon® Performance Solutions Vinyl Wire & Cable JKX202L PVC, Flexible  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Wire and Cable Grade

Material Notes: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.36 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 76
@Time 15.0 sec
ASTM D2240
Tensile Strength, Yield 13.8 MPaType IV, 510 mm/min; ASTM D638
Elongation at Break 300 %Type IV, 510 mm/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -42.0 °CASTM D746
Oxygen Index 30 %
@Thickness 1.91 mm
ASTM D2863
 
Processing PropertiesOriginal ValueComments
Melt Temperature 177 - 188 °C
 
Descriptive Properties
FeaturesFlame Retardant
FormsPellets
Lead Content<100 ppm
Processing MethodExtrusion Coating
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
Retention of Elongation, %90168 hr, UL Standard; 100°C, 889.0 µm
Retention of Tensile Strength, %110168 hr, UL Standard; 100°C, 889.0 µm
RoHS ComplianceRoHS Compliant
UsesCommunication Wire Jacketing
 Wire & Cable Applications
 Wire Jacketing
Wire TypesCATV

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PH1PN8935 / 102771

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.