MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Nouryon Accelerator 553SN Cobalt(II) 2-ethylhexanoate in solvent mixture
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Accelerator 553SN is a solution of 1.9% metal complexes for curing unsaturated polyester resins in combination with organic peroxide at room and elevated temperatures. Typically recommended for preacceleration of vinylester resins to avoid foaming during cure when using standard MEKP.

Applications: Accelerator 553SN is a solution of metal complexes, partly based on a cobalt salt in an organic solvent. Accelerator 553SN gives in comparison with the commonly used cobalt accelerator a much faster cure with comparable gel time. Accelerator 553SN is therefore very suitable where a faster demoulding time of the end product is required. Application areas are for instance: Gelcoat, RTM, production of polymer concrete. Accelerator 553SN can successfully be used for the production of cobalt pre-accelerated UP resins. The use of Accelerator 553SN will strongly reduce the gel time drift as observed with standard cobalt. Accelerator 553SN prevents foaming in VE resins with standard MEKP e.g. Butanox M-50.

CAS number 136-52-7

EINECS/ELINCS No.: 205-250-6

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.154 g/cc
 
Component Elements PropertiesOriginal ValueComments
Cobalt, Co 1.8 - 2.0 %
 
Descriptive Properties
AppearanceClear black/blue liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY005 / 285528

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.