MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis ME6032 Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ME6032 is a MDPE compound for solid insulation of telephone singles and data cables at high line speed. It contains a metal deactivator. Applications: Dry core and petroleum jelly filled cables. Specifications: ASTM D1248 Type II, Class A, Category 5, Grade E4, E5; BS 6234: Type 03; EN 50288; EN 50290-2-23; IEC 60708; ISO 1872-PE, KHN, 27-D003; NF C32-060; and DIN VDE 0207, 2Y11, 2Y12 and 2Y13.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.928 g/ccISO 1183
ESCR 100% Igepal® >= 250 hour
@Temperature 50.0 °C
F20; ASTM D1693-B
Thermal Stress Crack Resistance >= 1.00 hour
@Temperature 105 °C
IEC 60811-4-2/A
Oxidative Induction Time (OIT) 50 min
@Temperature 200 °C
IEC 60811-4-2/B
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 531s; ISO 868
Tensile Strength at Break 17.0 MPaISO 527
Elongation at Break 600 %ISO 527
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+6 ohm-cmIEC 60093
Dielectric Constant 2.3
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm
@Frequency 1000 Hz
IEC 60250
Dissipation Factor 0.00015
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -76.0 °CASTM D746
 
Processing PropertiesOriginal ValueComments
Processing Temperature 70.0 - 100 °Cconductor preheating temperature; 2400 m/min line speed
Middle Barrel Temperature 165 - 230 °C
Melt Temperature 220 - 240 °C
Head Temperature 230 °C
 
Descriptive Properties
Petroleum Jelly Absorption (%)8IEC 60811-4-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPC 1645 Polypropylene, Heterophasic Copolymer, Pipes
Borealis Daploy™ WB135HMS High Melt Strength Polypropylene for Foam Extrusion
Avient Trilliant™ HC HC5220-0040 RS Natural Polypropylene
Borealis Daploy™ WB180HMS Polypropylene
Borealis Daploy™ WB140HMS Polypropylene

PBOREA535 / 108794

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.