MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer ML7664 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN ML7664 polycarbonate (PC) siloxane resin, is a product targeting (profile) extrusion applications requiring extreme low temperature ductility. LEXAN ML7664 resin is a non-FR product available in opaque colors only.

Features: High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Density 1.19 g/ccISO 1183
Moisture Absorption 0.150 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %ISO 62-1
Viscosity 2.0 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0060 - 0.010 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 2.7 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 56.0 MPa50 mm/min; ASTM D638
 59.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 59.0 MPa50 mm/min; ISO 527
 60.0 MPa50 mm/min; ASTM D638
Elongation at Break 76 %50 mm/min; ISO 527
 86 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ASTM D638
 6.0 %50 mm/min; ISO 527
Tensile Modulus 2200 MPa5 mm/min; ASTM D638
 2300 MPa1 mm/min; ISO 527
Flexural Strength 90.0 MPayield, 2 mm/min; ISO 178
 97.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2100 MPa2 mm/min; ISO 178
 2300 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 847 JASTM D256
 710 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 64.0 kJ/m²80*10*4; ISO 180/1A
 54.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 77.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 72.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 125 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 127 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 143 °CRate B/50; ISO 306
 144 °CRate B/50; ASTM D1525
 145 °CRate B/120; ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 100 °CCalibrator Temperature
Zone 1 240 - 280 °CProfile Extrusion
Zone 2 260 - 290 °CProfile Extrusion
Zone 3 260 - 290 °CProfile Extrusion
Zone 4 260 - 290 °CProfile Extrusion
Adapter Temperature 270 - 300 °CProfile Extrusion
Die Temperature 260 - 290 °CProfile Extrusion
Melt Temperature 280 - 300 °CProfile Extrusion
Drying Temperature 120 °CProfile Extrusion
Dry Time 2.00 - 4.00 hourProfile Extrusion
Precipitation Temperature 100 - 120 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80409 / 288356

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.