Features PA 6 for injection moulding with addition of 5% graphite, the PA surface rolling resistance force is significantly lowered. Used mainly in the product of crates and cases for bearings, sliding bolts and slides. Delivered in black. Application: Injection Moulding Information Provided by Plastcom spol. s r.o. |