MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo EMERGE™ PC 8130-10 PC
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Product Description: EMERGE™ PC 8130-10 is a translucent, ultraviolet light resistance and ignition resistant PC resin. This resin contains no chlorinated, brominated or phosphate flame retardant additives and is intended to comply with global environmental standards. It combines mechanical performance and high heat resistance with excellent processing characteristics in injection molded applications. This resin contains mold release and it is UV stabilized.
Applications: Information technology equipment; Electronics and electrical appliances

Availability: Asia Pacific; Europe; North America

Additive: Mold Release; UV Stabilizer

Features: Bromine Free; Chlorine Free; Flame Retardant; Good Processability; High Heat Resistance; UV Resistant

Uses: Appliances; Electrical Housing; Electrical/Electronic Applications; Sheet; Thin-walled Parts

Appearance: Translucent

Form: Pellets

Processing Method: Injection Molding; Profile Extrusion

Information provided by Trinseo

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmASTM D955
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 8410 psiISO 527-2/50
 9430 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 8700 psi2.0 in/min; ASTM D638
 8700 psiISO 527-2/50
Elongation at Break 110 %ISO 527-2/50
 120 %2.0 in/min; ASTM D638
Elongation at Yield 6.0 %2.0 in/min; ASTM D638
 6.0 %ISO 527-2/50
Tensile Modulus 334000 psi0.039 in/min; ASTM D638
 348000 psiISO 527-1/1
Flexural Strength 13800 psi0.051 in/min; ASTM D790
 13800 psi0.079 in/min; ISO 178
Flexural Modulus 341000 psi0.079 in/min; ISO 178
 348000 psi0.051 in/min; ASTM D790
Izod Impact, Notched 13.0 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 33.0 ft-lb/in²ISO 180/1A
Charpy Impact, Notched 17.0 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmIEC 60093
Dielectric Strength 430 V/milIEC 60243-1
Dissipation Factor 0.0010
@Frequency 50 Hz
IEC 60250
 0.0020
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance <= 60 secASTM D495
Comparative Tracking Index 225 V
@Thickness 2.00 mm
Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 39.0 µin/in-°FISO 11359-2
 36.0 µin/in-°F
@Temperature -40.0 - 80.0 °C
ASTM D696
Hot Ball Pressure Test >= 257 °FIEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 291 °FAnnealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 257 °FUnannealed; ISO 75-2/A
 259 °FUnannealed; ASTM D648
 286 °FAnnealed; ISO 75-2/A
Vicat Softening Point 289 °FISO 306/B50
Flammability, UL94 V-0
@Thickness 1.52 mm
 V-0
@Thickness 3.05 mm
 5VA
@Thickness 3.05 mm
Oxygen Index 37 %ISO 4589-2
Glow Wire Ignition Temperature 1470 °F
@Thickness 2.03 mm
IEC 60695-2-13
Glow Wire Flammability Index 1760 °F
@Thickness 2.03 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 518 - 572 °F
Mold Temperature 140 - 230 °F
Drying Temperature 248 °F
Dry Time 3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTRINSE1524 / 312217

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.