Bayfol DF-A 1-2 900296 is a black colored Extrusion-Film based on Novodur (ABS), one side gloss, one side very fine matte. It has been specially developed for applications in the sector of decorative films, where Bayfol DF-A displays its excellent properties as a carrier material. Standard thickness: 500 µm other thicknesses on requestAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |