VESTOSINT 1164 white respectively 1174 white are nylon 12 fine powders which are specially developed for the minicoat process of small articles, e.g. corsetry or ferrit rings. VESTOSINT 1164 white and 1174 white are used additionally in paints.Information provided by Evonik |