Description: Capran® is a multipurpose nylon 6 film. Its physical properties are evenly distributed for optimum performance giving excellent resistance to flex cracking. It can be processed over a wide temperature range and exhibits outstanding abrasion resistance. Applications: Capron® Nylon Film is used in food packaging applications. Former Honeywell product; AdvanSix is a spin-off of Honeywell. |