Description/Features: - A Fluxed Blend
- Non-staining Stabilizer System
PolyOne First ChoiceDisclaimer: ProFlex is PolyOne's trademark for its brand of engineered elastomers. All ProFlex property data represents typical values and is not for specification purposes. Base Polymer: An un-accelerated, masterbatch compound based upon Bayer® Krynac® and/or Perbunan® brand NBR. Bayer®, Krynac®, and Perbunan® are trademarks of Bayer Corporation. ProFlex elastomeric compounds are manufactured in ISO 9002 registered facilities. Information provided by PolyOne Corporation. |