Morgan Advanced Materials announces the release of our new piezoelectric material, PZT-508-HD, for use in demanding transducer and actuator applications. The new, high density material was designed to achieve low porosity and a uniform microstructure, offering increased dielectric constant, low dielectric losses and improved electromechanical coupling coefficients. - High performance applications include medical imaging, inkjet printing and actuators.
- Higher dielectric permittivity and coupling results in higher sensitivity in imaging and other sensing applications.
- Significantly higher d31 yields higher displacement and blocked force in tube and bender applications.
- Improved mechanical properties resulting in improved machinability for generating finer features.
Information provided by Morgan Advanced Materials. Morgan's electroceramic business was sold to Ceramtec in 2018. |